ELASTOSAL SPM – Repair Kit


  • Base: polychloroprene
  • Yield: approx. 150 g/m²  per coat

Two component primer and protecting layer for the spatula compound ELASTOSAL ® SPM, hardener is necessary as second component.

Specifications ELASTOSAL
SPM
Base polychloroprene
Specific gravity 1,3 g/cm³
Oil resistance oil resistant according to DIN 53521
Shore hardness A approx. 65 ” (after complete curing)
Final hardening after approx. 24 h (at 20°C)
Primer / Protecting layer ELASTOSAL® SPM Primer + Hardener RE
Application spatula
Consumption [for 1 mm thickness] ≈ 1kg/m²
Temperature resistance up to 130° C, for a short time up to 150° C
Packing tin 500 g, 1 kg